Magnetization versus applied dc magnetic field data for Li0.7[Cr(pyz)2]Cl0.7·(THF)

  1. Perlepe, Panagiota 1
  2. Oyarzabal, Itziar 2
  3. Mailman, Aaron 3
  4. Yquel, Morgane 1
  5. Platunov, Mikhail 4
  6. Dovgaliuk, Iurii 5
  7. Rouzières, Mathieu 6
  8. Négrier, Philippe 7
  9. Mondieig, Denise 7
  10. Suturina, Elizaveta A. 8
  11. Dourges, Marie-Anne 9
  12. Bonhommeau, Sébastien 9
  13. Musgrave, Rebecca A. 10
  14. Pedersen, Kasper S. 11
  15. Chernyshov, Dmitry 5
  16. Wilhelm, Fabrice 4
  17. Rogalev, Andrei 4
  18. Mathonière, Corine 12
  19. Clérac, Rodolphe 6
  1. 1 Univ. Bordeaux, CNRS, Centre de Recherche Paul Pascal, UMR 5031, F-33600, Pessac, France & CNRS, Univ. Bordeaux, Bordeaux INP, ICMCB, UMR 5026, F-33600 Pessac, France.
  2. 2 Univ. Bordeaux, CNRS, Centre de Recherche Paul Pascal, UMR 5031, F-33600, Pessac, France & Chemistry Faculty, University of the Basque Country, UPV/EHU, 20018, Donostia-San Sebastián, Spain.
  3. 3 Department of Chemistry, University of Jyväskylä, P.O. Box 35, Jyväskylä, Finland.
  4. 4 ESRF-The European Synchrotron, CS 40220, F-38043 Grenoble Cedex 9, France.
  5. 5 Swiss-Norwegian Beamlines at the European Synchrotron Radiation Facility, F-38000 Grenoble, France.
  6. 6 Univ. Bordeaux, CNRS, Centre de Recherche Paul Pascal, UMR 5031, F-33600, Pessac, France
  7. 7 Univ. Bordeaux, CNRS, Laboratoire Ondes et Matière d'Aquitaine, UMR 5798, F-33400 Talence, France.
  8. 8 Department of Chemistry, University of Bath, BA2 7AY, UK.
  9. 9 Univ. Bordeaux, CNRS, Bordeaux INP, ISM, UMR 5255, F-33400 Talence, France.
  10. 10 Univ. Bordeaux, CNRS, Centre de Recherche Paul Pascal, UMR 5031, F-33600, Pessac, France.
  11. 11 Univ. Bordeaux, CNRS, Centre de Recherche Paul Pascal, UMR 5031, F-33600, Pessac, France & Department of Chemistry, Technical University of Denmark, DK-2800 Kgs. Lyngby, Denmark.
  12. 12 CNRS, Univ. Bordeaux, Bordeaux INP, ICMCB, UMR 5026, F-33600 Pessac, France.

Editor: Zenodo

Año de publicación: 2020

Tipo: Dataset

CC BY 4.0

Resumen

Magnetization versus applied dc magnetic field data in the –7 to 7 T field range from 1.85 K to 520 K for Li<sub>0.7</sub>[Cr(pyz)<sub>2</sub>]Cl<sub>0.7</sub>·(THF). The data are provided in a tab-delimited text format.